The Journal of the American Dental Association
HOME HELP FEEDBACK SUBSCRIPTIONS ARCHIVE SEARCH TABLE OF CONTENTS
 QUICK SEARCH:   [advanced]


     


J Am Dent Assoc, Vol 135, No 5, 587-594.
© 2004 American Dental Association

This Article
Right arrow Full Text
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Download to citation manager
Right arrow reprints & permissions
Citing Articles
Right arrow Citing Articles via Google Scholar
Google Scholar
Right arrow Articles by PATEL, S. B.
Right arrow Articles by SHEN, C.
Right arrow Search for Related Content
PubMed
Right arrow PubMed Citation
Right arrow Articles by PATEL, S. B.
Right arrow Articles by SHEN, C.
Related Collections
Right arrow Esthestics

RESEARCH

JADA Continuing Education

The effect of surface finishing and storage solutions on the color stability of resin-based composites



SHREENA B. PATEL, VALERIA V. GORDAN, D.D.S., M.S., ALLYSON A. BARRETT and CHIAYI SHEN, Ph.D.

Background. The authors tested the hypothesis that surface-finishing treatments and the type of storage solutions significantly affected the staining of resin-based composites, or RBCs, and unfilled resins, or URs.

Methods. Fifty-four RBC and 54 UR disks were polymerized through a polyester film strip (Mylar, DuPont, Wilmington, Del.) and polished in one of three groups: 1-micrometer aluminum oxide, 15-µm diamond plate and no treatment (polyester film). All specimens were immersed in water for two days and then in coffee, cola or red wine for seven more days at 37 C. The authors recorded tristimulus color measurements before the immersions; after one and two days in water; and after one, two, three and seven days in the storage solutions.

Results. Most of the color changes occurred between day 2 in water and day 7 in the staining solution. Analysis of variance showed that the finishing treatment and storage solution significantly influenced the overall color change ({Delta}E), and interactions occurred between the finishing treatment and the storage solution (P < .0001) for both materials. RBC specimens generally exhibited greater color changes than did UR specimens. The polyester film finishing exhibited the greatest amount of color change, while the diamond finishing exhibited the least amount of color change. Immersion in wine caused the greatest color change for both materials; cola and coffee resulted in the smallest color change for RBC and UR specimens, respectively.

Conclusions. Finishing treatments and storage solutions significantly affect the surface staining of RBC materials. Polyester film finishing and red wine produced the greatest color change after seven days for RBC specimens.

Clinical Implications. Clinicians should remove the polyester film–finished surface and advise patients that drinking wine could intensify surface staining on RBC restorations.







HOME HELP FEEDBACK SUBSCRIPTIONS ARCHIVE SEARCH TABLE OF CONTENTS
Copyright©1995-2004 American Dental Association (ADA).
Reproduction or republication strictly prohibited without prior written permission of ADA.